Grade : | 19MnB4 | |
Number: | 1.5523 | |
Standard: |
| |
Classification: | Alloy special steel | |
Equivalent grades: | Go here |
Chemical composition % of grade 19MnB4 (1.5523)
C | Si | Mn | P | S | Al | B |
0.17 - 0.24 | max 0.4 | 0.8 - 1.15 | max 0.035 | max 0.035 | max 0.02 | 0.0008 - 0.005 |
Mechanical properties of grade 19MnB4 (1.5523)
Rm - Tensile strength (MPa) (+AC) | 520 |
Nominal thickness (mm): | to 16 |
Rm - Tensile strength (MPa) (+QT) | 800-950 |
Nominal thickness(mm): | to 16 |
Rp0.2 0.2% proof strength (MPa) (+QT) | 640 |
Temperature ° C | +20 |
KV - Impact energy (J) (+QT) | 40 |
Nominal thickness (mm): | to 16 |
A - Min. elongation at fracture (%) (+QT) | 14 |
Z - Reduction in cross section on fracture (%) (+AC) | 64 |
Nominal thickness (mm): | to 16 |
Z - Reduction in cross section on fracture (%) (+QT) | 52 |
Equivalent grades of grade 19MnB4 (1.5523)
France AFNOR | |
|
Mechanical properties
Mechanische Eigenschaften
Caracteristiques mecaniques
ReH | Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d锟絜lasticite minimale |
Rm | Tensile strength / Zugfestigkeit / Resistance a la traction |
A | Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal |
J | Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc |
Heat treatment conditions
+A | Soft annealed |
+AC | Annealed to achieve spheroidization of the carbides |
+AR | As rolled |
+AT | Solution annealed |
+C | Cold drawn |
+CR | Cold rolled |
+FP | Treated to ferrite-pearlite structure and hardness range |
+LC | Skin passed |
+N | Normalized |
+NT | Normalized and tempered |
+P | Precipitation hardened |
+QA | Air quenched and tempered |
+QL | Liquid quenched and tempered |
+QT | Quenched and tempered |
+S | Treated to improve shearability |
+SH | As rolled and turned |
+SR | Cold drawn and stress relieved |
+TH | Treated to hardness range |
Properties of 19MnB4 (1.5523). Hardness of 19MnB4 (1.5523). Strength of 19MnB4 (1.5523). Elongation of 19MnB4 (1.5523).